Grade |
Chemical composition(%) | ||||||
| ERNiCrFe-7 | C | Mn | Si | S | P | Mo | Ni |
| ≤0.02 | ≤1.0 | ≤0.5 | ≤0.03 | ≤0.04 | 15~17 | Bal | |
| W | Cu | V | Fe | Others | Cr | Co | |
| 3.0~4.5 | ≤0.5 | ≤0.35 | 4~7 | <0.5 | 14.5~16.5 | ≤2.5 | |
Mechanical properties
| Tensile Strength | Yield Strength | Elongation |
| 790Mpa | 590Mpa | 27% |
Welding paramaters
| Process | Diameter |
Voltage |
Amperage |
Gas |
| TIG | .045” (1.2mm) |
13-16 |
80-110 |
100% Argon |
| 1/16” (1.6mm) |
14-18 |
90-130 |
100% Argon |
|
| 3/32” (2.4mm) |
15-20 |
120-175 |
100% Argon |
|
| 1/8” (3.2mm) |
15-20 |
150-220 |
100% Argon |
|
| MIG | .045” (1.2mm) |
28-32 |
180-220 |
75% Argon + 25% Helium |
| 1/16” (1.6mm) |
29-33 |
200-250 |
75% Argon + 25% Helium |
|
| 3/32” (2.4mm) |
28-30 |
275-350 |
Suitable Flux may be used |
|
| SAW | 1/8” (3.2mm) |
29-32 |
350-450 |
Suitable Flux may be used |
| 5/32” (4.0mm) |
30-33 |
400-550 |
Suitable Flux may be used |